Material properties: Tensile strength 26.2 MpaASTM Flexural strength 99 MpaASTM Flexural modulus 2640 MpaASTM Shore hardness 76.75 DASTM Density 1.1 g/cm3 at 23 CASTM Viscosity 200-225 mPa.s at 23 CDIN Color Light pink Post process: 1- Washing After the printing is completed, wash the part as attached to the building plate with ethyl alcohol (>%90) or isopropyl alcohol (>%90) for 5 minutes. Make sure that alcohol covers the part entirely when washing. Use a brush to remove uncured resin if needed. Do not over-wash, it may cause deterioration in dimensions of the part. 2- Drying Use air-compressor to dry the washed part. Make sure that the part is dry and uncured resin is cleaned up completely. If still uncured resin left on the part, wash it with fresh alcohol and dry again. 3- Part Removal Remove the printed part from the building plate using a scraping tool. Be very careful not to damage the model. 4- Post Curing You can reach 99 MPa flexural strength after curing Please cure 20 minutes with MEDIFIVE curing chamber at 3rd-degree light intensity Otoflash curing recommendations; 10000 flashes without gas. After post curing, supports should be removed from the model cautiously. Storage conditions: Store the PowerResins Model bottle in dark and moisture free place at room temperature (20-24 °C). Do not forget shaking the resin well before use. If your printer has heater, you can set the temperature at 32 °C. Otherwise, you can heat your resin in a microwave for 18 seconds or by submerging in hot water for 15-20 minutes.
Have a question about this?
We currently ship within the US, with more countries coming soon.
Final cost and dates are confirmed at checkout.
🇺🇸 Ship from USA · On Agora since 2025
$150.00